Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 171 GPa | 24800 ksi | calculated |
Ceradyne CeraTrex™ 146-IS Silicon Carbide Features:high puritycorrosion resistancewear resistanceApplications:semiconductor componentssputtering targetsInformation provided by Ceradyne Company |