Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.160 GPa | 23.2 ksi | ASTM C273 |
3A Composites Core Materials BALTEK® SB.100 Structural End-Grain Balsa BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent b.. |