Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 23.0 GPa | 3340 ksi | calculated |
Piezo Kinetics 552 Lead Zirconate Titanate Piezoelectric Denoted as Navy Type VI, this ceramic is used as sensors that require extremely high dielectric constant and large displacements. PKI 556 material has been slightly modified to give a higher g33 val.. |
|||
Shear Modulus | 23.0 GPa | 3340 ksi | calculated |
Piezo Kinetics 906 Lead Nickel Niobate Piezoelectric PKI 906 is slightly different in composition than the "general" PZT formulations. Its PZT-doped Lead Nickel Niobate composition was developed to enhance the d33 and dielectric properties of Navy Typ.. |
|||
Shear Modulus | 23.0 GPa | 3340 ksi | calculated |
Schott F2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 23.0 GPa | 3340 ksi | calculated |
Schott F2HT Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 23.0 GPa | 3340 ksi | calculated |
Schott P-PK53 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 23.0 GPa | 3340 ksi | calculated |
Schott SF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 23.0 GPa | 3340 ksi | calculated |
Schott SF4 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 23.0 GPa | 3340 ksi | calculated |
Schott SF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
Shear Modulus | 23.0 GPa | 3340 ksi | calculated |
Schott SF56A Glass Information Provided by SCHOTT North America, Inc. |