Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.45 GPa | 210 ksi | ISO 6721-2 |
Styrolution Polystyrol 168 N GR 2 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Shear Modulus | 1.45 GPa | 210 ksi | ISO 6721-2 |
Styrolution Polystyrol 168 N GR 21 PS Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact.. |
|||
Shear Modulus | 1.45 GPa | 210 ksi | Plate Shear, L Direction, typ |
Hexcel® HexWeb® CR III 1/16-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |