Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.38 GPa | 200 ksi | Calculated |
SABIC Innovative Plastics Ultem 1000M PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Shear Modulus | 1.38 GPa | 200 ksi | Calculated |
SABIC Innovative Plastics Ultem 1000M PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |