Polymer Property : Shear Modulus = 20.9 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 20.9 GPa
3030 ksi
Calculated
Schott Glass 8337B Borosilicate Glass
Borosilicate glass for sealing to Kovar metal and tungsten, highly UV-transmitting photomultiplier and UV detectors The heavy metal content for the elements lead, cadmium, mercury, and hexavalent ..
Shear Modulus 20.9 GPa
3030 ksi
Calculated
Corning 7070 Lithia Potash Borosilicate Crushed/Powdered Glass
Available in mesh sizes 4 through 325 and can be customized. Devitrifies before reaching a softening point. Used for sealing and other applications.Information provided by Corning Incorporated.