Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 2.78 GPa | 403 ksi | Calculated |
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension.. |