Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.0160 GPa | 2.32 ksi | average; ASTM C393 |
3A Composites Core Materials AIREX® C70.48 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |