Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.27 GPa | 184 ksi | Calculated |
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix HexPly® M18 has been developed to fulfill the requirements of the aerospace industry for primary structures using standard manufacturing processes. The matrix has improved properties which allow ea.. |