Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.130 GPa | 18.9 ksi | |
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Shear Modulus | 0.130 GPa | 18.9 ksi | Plate Shear, W direction |
Hexcel® HexWeb® CRF-1/4-ACG-.002-3.4 Chromate free ACG® Honeycomb Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app.. |