Polymer Property : Shear Modulus = 17700 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 122 GPa
17700 ksi
calculated
Ceradyne Ceralloy® 147-1E Silicon Nitride
Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradynes ..
Shear Modulus 122 GPa
17700 ksi
Calculated
Ceradyne Ceralloy® 147-31N Sintered Reaction Bonded Silicon Nitride (Si3N4)
Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met..
Shear Modulus 122 GPa
17700 ksi
Calculated
CeramTec Rubalit® IS 95 Brown Alumina
Rubalit® IS 95 brown is a high-performance alumina ceramic. Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at..