Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 12.0 GPa | 1740 ksi | average; ASTM C393 |
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |
|||
Shear Modulus | 12.0 GPa | 1740 ksi | |
Mateck Thallium Bromoiodide TIBr-TII (KRS-5) Optical crystals |