Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 162 GPa | 23500 ksi | Calculated |
M Cubed Technologies SSC-802 Reaction-Bonded Silicon Carbide Medium-grained reaction-bonded SiC for high wear applications. Bullnoses, fan liners, hydrocyclone liners, etc. Can be cast into very large shapes (greater than 4 ft. square, 5-6 inches thick)Info.. |
|||
Shear Modulus | 162 GPa | 23500 ksi | Calculated |
CeramTec Rocar® SiG Silicon Carbide, SiSiC Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch.. |