Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 154 GPa | 22300 ksi | Calculated |
M Cubed Technologies SSC-903 Reaction-Bonded Silicon Carbide Coards-grained reaction-bonded SiC for high wear applications. Bullnoses, fan liners, hydrocyclone liners, etc. Can be cast into very large shapes (greater than 4 ft. square, 5-6 inches thick)Info.. |