Shear Modulus 0.827 - 1.03 GPa
120 - 149 ksi
Average value: 0.922 GPa Grade Count:11
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..