Polymer Property : Shear Modulus = 144 GPa
Polymer Property :
Shear Modulus =
144 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Shear Modulus
144
GPa
20900
ksi
Calculated
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2
DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications.