Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.100 GPa | 14.5 ksi | Plate Shear, W direction |
Hexcel® HexWeb® CRF-1/2-ACG-.003-2.6 Chromate free ACG® Honeycomb Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app.. |
|||
Shear Modulus | 0.100 GPa | 14.5 ksi | Plate Shear, W Direction, typ, preliminary value obtained at .500 inch thickness |
Hexcel® HexWeb® HRH-327 - 1/8 - 5.5 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |