Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 131 GPa | 19000 ksi | Calculated |
CeramTec B 601 Alumina, 98.5% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |
|||
Shear Modulus | 131 GPa | 19000 ksi | Calculated |
CeramTec Rubalit® A 1894 Alumina, 94% Rubalit® A 1894 (94%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond .. |
|||
Shear Modulus | 131 GPa | 19000 ksi | Calculated |
CoorsTek SC-DSG (SC-35) Graphite Loaded Sintered Silicon Carbide Thermal Shock Delta Tc = 600°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Shear Modulus | 131 GPa | 19000 ksi | calculated |
Ceradyne Ceralloy® 1370-1E Aluminum Nitride Features:standard grade Applications:semiconductor componentsInformation provided by Ceradyne Company |
|||
Shear Modulus | 131 GPa | 19000 ksi | calculated |
Ceradyne Ceralloy® 1370DP Aluminum Nitride Features:high thermal conductivityApplications:semiconductor componentsmicrowave componentsInformation provided by Ceradyne Company |
|||
Shear Modulus | 131 GPa | 19000 ksi | |
CeramTec 975 Alumina, 99.5% 975 (99.5%) offers unique technology by virtue of its optimal dispersion of the MgO phase with the alumina grains. With virtually no transgranular porosity in its microstructure, 975 exhibits high d.. |