Mechanical Properties Metric English Comments
Shear Modulus 126 GPa
18300 ksi
Calculated
Ceradyne Ceralloy® 147-A Hot Pressed Silicon Nitride (Si3N4)
Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met..
Shear Modulus 126 GPa
18300 ksi
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2
950 has a combination of high strength (from zirconia) and high hardness (from the alumina phase). It has excellent wear resistance, both in sliding and abrasive conditions. This material offers a g..