Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 84.2 GPa | 12200 ksi | Calculated |
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy This alloy consists of 65% Be and 35% Al (by weight) and is used primarily for moderate strength cast electronic and thermal packaging applications. BeAl-191 also provides a unique capability for se.. |
|||
Shear Modulus | 84.2 GPa | 12200 ksi | Calculated |
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65%.. |
|||
Shear Modulus | 84.0 GPa | 12200 ksi | dynamic |
Materion AlBeCastâ„¢ IC910 Aluminum Beryllium Composite Mechanical properties are typical values at RT. AlBeCastâ„¢ IC910 is an aluminum-beryllium alloy that combines the advantages of a net shape casting technology, investment casting, with the stif.. |