Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 78.0 GPa @Temperature 20.0 °C |
11300 ksi @Temperature 68.0 °F |
|
Industeel VIRGO 39 16% Cr, 5% Ni, Martensitic Stainless Steel Description: Virgo 39 is a 16% Cr, 5% Ni, 1% Mo low carbon martensitic stainless steel. The grade is specially designed to combine high mechanical properties including toughness and improved corrosi.. |
|||
Shear Modulus | 78.0 GPa | 11300 ksi | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725) Age Hardened Strip Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Strip samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Shear Modulus | 78.0 GPa | 11300 ksi | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Round Tensile strength (ultimate and yield), hardness, impact, and elongation values reported here are typical for Age Hardened Round samples. Other property values are typical of INCONEL® alloy 725.D.. |
|||
Shear Modulus | 78.0 GPa | 11300 ksi | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Age Hardened Tube Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Age Hardened Tube samples. Other property values are typical of INCONEL® alloy 725.Data provi.. |
|||
Shear Modulus | 78.0 GPa | 11300 ksi | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Round Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Round samples. Other property values are typical of INCONEL® alloy 725.Data provided.. |
|||
Shear Modulus | 78.0 GPa | 11300 ksi | |
Special Metals INCONEL® 725 Nickel Superalloy (UNS N07725), Annealed Tube Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Tube samples. Other property values are typical of INCONEL® alloy 725.Data provided .. |
|||
Shear Modulus | 78.0 GPa | 11300 ksi | torsion |
AK Steel 301 Austenitic Stainless steel AK Steel 301 provides high strength and good ductility when cold worked. It is a modification of AK Steel 302 to increase the cold work-hardening range, to permit higher tensile strengths to be ach.. |
|||
Shear Modulus | 78.0 GPa | 11300 ksi | torsion |
AK Steel 304 Austenitic Stainless steel AK Steel 304 is a variation of the basic 18-8 grade, Type 302. Lower carbon, in Type 304, minimizes chromium carbide precipitation due to welding and its susceptibility to intergranular corrosion. .. |
|||
Shear Modulus | 78.0 GPa | 11300 ksi | torsion |
AK Steel 304L Austenitic Stainless steel AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive co.. |
|||
Shear Modulus | 78.0 GPa | 11300 ksi | torsion |
AK Steel 321 Austenitic Stainless steel AK Steel 321 is a stabilized austenitic stainless steel similar to Type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 427 .. |
|||
Shear Modulus | 77.8 GPa | 11300 ksi | Calculated |
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use.. |