Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 113 GPa | 16400 ksi | Ultrasonic |
CeramTec 771 94% Alumina (Al2O3) Te value is 840°C. Hasselman Thermal Shock value is 200 K.Data provided by CeramTec North America. |
|||
Shear Modulus | 113 GPa | 16400 ksi | Calculated |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |