Mechanical Properties Metric English Comments
Shear Modulus 0.260 - 0.730 GPa
37.7 - 106 ksi
Average value: 0.541 GPa Grade Count:20
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..