Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.42 - 1.70 GPa | 206 - 247 ksi | Average value: 1.54 GPa Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Shear Modulus | 0.629 - 1.70 GPa | 91.2 - 247 ksi | Average value: 1.08 GPa Grade Count:6 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |