Shear Modulus >= 0.0108 GPa

@Temperature -100 - 200 °C
>= 1.57 ksi

@Temperature -148 - 392 °F
Average value: 1.02 GPa Grade Count:2
Overview of materials for Nylon 6, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea..