Polymer Property : Shear Modulus = 1.21 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 1.21 GPa
175 ksi
Plate Shear, L Direction, typ, preliminary
Hexcel® HexWeb® CR III 1/8-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Shear Modulus 1.21 GPa
175 ksi
Calculated
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM
Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity..