Shear Modulus 1.09 GPa
158 ksi
Calculated
Hexcel® HexPly® 954-2A Curing Cyanate Resin
HexPly® 954-2A is a 350°F (177°C) curing toughened cyanate resin with low moisture absorption, and excellent microcracking resistance. HexPly® 954-2A is formulated for autoclave or press molding..