Shear Modulus 0.00690 GPa
1.00 ksi
Typical; ASTM C273
Parabeam Industrie Paraglass 12 3D Glass Fabric
Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl..
Shear Modulus >= 0.00689 GPa
>= 1.00 ksi
Plate Shear, W Direction, minimum individual
Hexcel® HexWeb® HRH-310 - 1/8 - 1.8 Aramid Fiber/Polyimide Resin Honeycomb
Designation: Material-Cell Size-DensityHexWeb HRH-310 is manufactured from aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the hexagon..