Shear Modulus 0.00640 - 0.307 GPa
0.928 - 44.5 ksi
Average value: 0.0954 GPa Grade Count:12
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..