Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.920 GPa | 133 ksi | DIN 53457 |
Global PP-1140-T Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-disposable drinkware, thin-walled partsInformation provided by Global Polymers Corporation. |
|||
Shear Modulus | 0.920 GPa | 133 ksi | ISO 6721-2 |
Styrolution Luran® S KR 2863 C Colored ASA+PC Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Shear Modulus | 0.920 GPa | 133 ksi | |
Cymat A35620SC 040SS Stabilized Aluminum Foam Description: Cymat A35620SC 040SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.4 g/cm3. The mechanical properties of SAF make it .. |
|||
Shear Modulus | 0.920 GPa | 133 ksi | ISO 6721-2 |
Styrolution Luran® S KR 2863 C UV Colored ASA+PC Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |