Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.590 GPa | 85.6 ksi | DIN 53457 |
Global PP-3240-H Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-sheets, bottlesInformation provided by Global Polymers Corporation. |
|||
Shear Modulus | 0.590 GPa | 85.6 ksi | DIN 53457 |
Global PP-2300-NC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-furniture, crates, closures, electrical appliances, automotiveInformation provided by Global Polyme.. |