Mechanical Properties Metric English Comments
Shear Modulus 0.356 GPa
51.6 ksi
ribbon direction
Ultracor® UCF-355-3/8-3.5 Honeycomb Core Material
Construction: ±45° T300. Fiber: Carbon T300. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be use..