Mechanical Properties Metric English Comments
Shear Modulus 0.331 GPa
48.0 ksi
ribbon direction
Ultracor® UCF-51-3/8-2.0 Honeycomb Core Material
Construction: ±45° XN50. Fiber: Carbon XN50. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be use..