Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | >= 0.147 GPa @Temperature -50.0 - 200 °C |
>= 21.3 ksi @Temperature -58.0 - 392 °F |
Average value: 1.10 GPa Grade Count:1 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |