Mechanical Properties Metric English Comments
Shear Modulus 0.0669 GPa
9.70 ksi
Plate Shear, L Direction, typical value
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 2.5 Aramid Honeycomb
Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod..