Polymer Property : Shear Modulus = 0.0228 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.0228 GPa
3.30 ksi
Plate Shear, L Direction
Hexcel® HexWeb® HRH-36/OX - 3/16 - 2.0 Para-Aramid/Phenolic Core
Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low..
Shear Modulus >= 0.0228 GPa
>= 3.30 ksi
Plate Shear, L Direction, minimum avg.
Hexcel® HexWeb® HRH-310 - 1/8 - 1.8 Aramid Fiber/Polyimide Resin Honeycomb
Designation: Material-Cell Size-DensityHexWeb HRH-310 is manufactured from aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the hexagon..