Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | >= 0.0210 GPa @Temperature -50.0 - 250 °C |
>= 3.05 ksi @Temperature -58.0 - 482 °F |
Average value: 1.00 GPa Grade Count:4 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Shear Modulus | 0.0210 GPa | 3.05 ksi | average; ASTM C393 |
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Shear Modulus | 0.0210 GPa | 3.05 ksi | average; ASTM C393 |
3A Composites Core Materials AIREX® T92.100 Easy Processing Structural Foam AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,.. |