Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.009915 GPa | 1.438 ksi | ASTM D412 Method A |
Seals Eastern 7204 Ethylene-Propylene Rubber Y267-Type EPDM for geothermal steam service. Ultra-Low compression set.Information provided by Seals Eastern, Inc. |