Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 0.00500 GPa | 0.725 ksi | ASTM C393 |
3A Composites Core Materials AIREX® C51.60 Industrial Processing Foam AIREX® C51 is a closed-cell polymer foam with outstanding damage tolerance and formability. Its excellent price / performance ratio uniquely qualifies this core material for high-volume sandwich .. |