Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 0.00193 GPa
0.280 ksi
ASTM D412 Method A
Seals Eastern 5862 Fluoro-silicone
Fluoro-siliconeInformation provided by Seals Eastern, Inc.
Shear Modulus 0.00193 - 0.0243 GPa
0.280 - 3.53 ksi
Average value: 0.00760 GPa Grade Count:19
Overview of materials for Thermoset Fluoroelastomer
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Fluoroelastomer". Each property range of values reported is minimum and maximum values of appr..