Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 10.6 MPa-m½ | 9.65 ksi-in½ | |
PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |