Polymer Property : Fracture Toughness = 8.10 MPa-m½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 8.10 MPa-m½
7.37 ksi-in½
K<sub>IC</sub> (SEVNB); DIN CEN/TS 14425-1
CeramTec ZN 40 Zirconia, ZrO2-MgO
ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma..