Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 8.00 - 10.0 MPa-m½ | 7.28 - 9.10 ksi-in½ | |
China-Yixing Longly Refractories Zirconia Ceramics LONGLY provides a multitude of zirconia products including balls, plates, tubes, rods and etc. by adopting magnesia, calcia or yttria stabilized zirconia powder as raw material through dry pressing,.. |