Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 7.60 MPa-m½ | 6.92 ksi-in½ | Average K<sub>IC</sub>. |
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |