Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 65.0 - 69.0 MPa-m½ | 59.2 - 62.8 ksi-in½ | K(IC); Typical Bar (heat treatment unspecified); Longitudinal |
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |
|||
Fracture Toughness | 65.0 - 69.0 MPa-m½ | 59.2 - 62.8 ksi-in½ | K(IC); Typical Bar (heat treatment unspecified); Longitudinal |
TIMET TIMETAL® 550 (Ti-4Al-4Mo-2Sn) Titanium Alloy Solution Treated and Aged High-Strength Forging AlloyIndustry Specifications: Germany Aerospace: 3.7184. France: T-A4DE. UK Aerospace Specifications BS TA. 45, 46, 47, 48,49, 50, 51, 57.Features: TIMETAL 550, like TIMETAL.. |