Polymer Property : Fracture Toughness = 5.01 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 5.50 MPa-m½
5.01 ksi-in½
ASTM C1421
M Cubed Technologies HSC-702 Aluminum-toughened Reaction Bonded Silicon Carbide
High fracture tougness reaction bonded SiC. Used in applications that require both high wear and high impact resistance. Bullnoses, fan liners, hydrocyclone liners, etc.Information provided by M C..
Fracture Toughness 5.50 MPa-m½
5.01 ksi-in½
K<sub>IC</sub> (SEVNB); DIN CEN/TS 14425-1
CeramTec SL 303 Silicon Nitride, SiAION+SiC
SL 303 is a silicon nitride ceramic. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile i..