Mechanical Properties Metric English Comments
Fracture Toughness 4.90 MPa-m½
4.46 ksi-in½
K<sub>IC</sub> (SEVNB); DIN CEN/TS 14425-1
CeramTec B 601 Alumina, 98.5%
Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures.