Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 3.00 - 4.00 MPa-m½ | 2.73 - 3.64 ksi-in½ | Notched Beam |
CoorsTek AD-85 Alumina (nom. 85% Al2O3) Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Fracture Toughness | 3.00 - 4.00 MPa-m½ | 2.73 - 3.64 ksi-in½ | Notched Beam |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Fracture Toughness | 3.00 - 4.00 MPa-m½ | 2.73 - 3.64 ksi-in½ | Klc; Notched Beam |
CoorsTek ADD-96 96% Alumina |
|||
Fracture Toughness | 3.00 - 4.00 MPa-m½ | 2.73 - 3.64 ksi-in½ | Klc; Notched Beam |
CoorsTek Boron Carbide Reaction-Bonded Boron Carbide Lowest density for ultra-lightweight designs |