Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 3.51 MPa-m½ | 3.19 ksi-in½ | |
Hexcel® HexPly® 8551-7 Epoxy Matrix HexPly® 8551-7 is an amine-cured, toughened epoxy resin system supplied with unidirectional graphite fibers. Typical reinforcement is continuous IM7 (intermediate modulus) graphite filaments. HexPl.. |