Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 18.0 - 20.0 MPa-m½ | 16.4 - 18.2 ksi-in½ | |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |
|||
Fracture Toughness | 18.0 - 20.0 MPa-m½ | 16.4 - 18.2 ksi-in½ | |
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part.. |